Polymer Property : Thermal Conductivity = 0.368 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0530 W/m-K

@Temperature 700 °C
0.368 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Unifrax Excelfrax® 1900 Panel Microporous Insulation
Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo..
Thermal Conductivity 0.0530 W/m-K

@Temperature 130 °C
0.368 BTU-in/hr-ft²-°F

@Temperature 266 °F
3M Novec™ 7500 Engineered Fluid
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a..