Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0320 W/m-K @Temperature 400 °C |
0.222 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Unifrax Excelfrax® 1900 Panel Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |