Thermal Properties Metric English Comments
Thermal Conductivity 0.0320 W/m-K

@Temperature 400 °C
0.222 BTU-in/hr-ft²-°F

@Temperature 752 °F
Unifrax Excelfrax® 1900 Panel Microporous Insulation