Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.164 W/m-K @Temperature 37.8 °C |
1.14 BTU-in/hr-ft²-°F @Temperature 100 °F |
|
Duratherm G Polyalkylenev Glycol Heat Transfer Fluid Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improv.. |