Material Notes:
Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improved clarity.Information provided by Duratherm.
Physical Properties Metric English Comments
Specific Gravity 0.963 g/cc
0.963 g/cc
at 60°F
Density 0.787 g/cc

@Temperature 260 °C
0.0284 lb/in³

@Temperature 500 °F
0.819 g/cc

@Temperature 204 °C
0.0296 lb/in³

@Temperature 400 °F
0.923 g/cc

@Temperature 37.8 °C
0.0333 lb/in³

@Temperature 100 °F
Kinematic Viscosity 1.35 cSt

@Temperature 260 °C
1.35 cSt

@Temperature 500 °F
Kinematic Viscosity at 40°C (104°F) 34 cSt
34 cSt
Kinematic Viscosity at 100°C (212°F) 7.1 cSt
7.1 cSt
Vapor Pressure 0.0103 bar

@Temperature 204 °C
7.75 torr

@Temperature 400 °F
0.01517 bar

@Temperature 260 °C
11.38 torr

@Temperature 500 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.97 J/g-°C

@Temperature 37.8 °C
0.470 BTU/lb-°F

@Temperature 100 °F
2.30 J/g-°C

@Temperature 204 °C
0.550 BTU/lb-°F

@Temperature 400 °F
2.34 J/g-°C

@Temperature 260 °C
0.560 BTU/lb-°F

@Temperature 500 °F
Thermal Conductivity 0.131 W/m-K

@Temperature 260 °C
0.912 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.138 W/m-K

@Temperature 204 °C
0.960 BTU-in/hr-ft²-°F

@Temperature 400 °F
0.164 W/m-K

@Temperature 37.8 °C
1.14 BTU-in/hr-ft²-°F

@Temperature 100 °F
Pour Point -40.0 °C
-40.0 °F
Flammability Test 543
543
Fire Point, °F
704
704
Autoignition Temp, °F
Flash Point 266 °C
511 °F
Descriptive Properties Value Comments
Max Bulk Temp (°F) 500
Max Film Temp (°F) 550