Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.145 W/m-K @Temperature 500 °C |
1.01 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |