Polymer Property : Thermal Conductivity = 1.01 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.145 W/m-K

@Temperature 500 °C
1.01 BTU-in/hr-ft²-°F

@Temperature 932 °F
3M Nextel™ AF-30 Industrial Woven Fabric 312
Information provided by 3M