Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.126 W/m-K @Temperature 316 °C |
0.876 BTU-in/hr-ft²-°F @Temperature 600 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |