Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0159 W/m-K @Temperature 538 °C |
0.110 BTU-in/hr-ft²-°F @Temperature 1000 °F |
8 pcf blanket (Parallel to Thickness) |
Zircar Ceramics ASB-2600 Alumina-Silica Blanket Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |