Material Notes:
Useful to temperatures of 1400°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 2.76 g/cc
0.0997 lb/in³
Filament Diameter 6.0 µm
6.0 µm
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C

@Temperature 1100 °C
0.280 BTU/lb-°F

@Temperature 2010 °F
Thermal Conductivity 0.0159 W/m-K

@Temperature 538 °C
0.110 BTU-in/hr-ft²-°F

@Temperature 1000 °F
8 pcf blanket (Parallel to Thickness)
0.0259 W/m-K

@Temperature 816 °C
0.180 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf blanket (Parallel to Thickness)
0.0500 W/m-K

@Temperature 260 °C
0.347 BTU-in/hr-ft²-°F

@Temperature 500 °F
8 pcf blanket (Parallel to Thickness)
0.290 W/m-K

@Temperature 1093 °C
2.01 BTU-in/hr-ft²-°F

@Temperature 1999 °F
8 pcf blanket (Parallel to Thickness)
Maximum Service Temperature, Air 1427 °C
2601 °F
Shrinkage 2.10 %

@Temperature 1260 °C,
Time 90000 sec
2.10 %

@Temperature 2300 °F,
Time 25.0 hour
8 pcf blanket (Perpendicular to Thickness)
2.60 %

@Temperature 1315 °C,
Time 90000 sec
2.60 %

@Temperature 2399 °F,
Time 25.0 hour
5.10 %

@Temperature 1426 °C,
Time 90000 sec
5.10 %

@Temperature 2599 °F,
Time 25.0 hour
8 pcf blanket (Perpendicular to Thickness)
Component Elements Properties Metric English Comments
Al2O3 >= 51 %
>= 51 %
Other <= 2.0 %
<= 2.0 %
SiO2 47 %
47 %
Descriptive Properties Value Comments
Color White
Fiber Length 4-7 in