Thermal Properties Metric English Comments
Thermal Conductivity 0.0830 W/m-K

@Temperature 260 °C
0.576 BTU-in/hr-ft²-°F

@Temperature 500 °F
Duratherm S Silicone Heat Transfer Fluid
Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s..
Thermal Conductivity 0.0830 W/m-K

@Temperature -70.0 °C
0.576 BTU-in/hr-ft²-°F

@Temperature -94.0 °F
3M Novec™ 7500 Engineered Fluid
3M™ Novec™ 7500 is a non-flammable fluid with a very low global warming potential (GWP.) Its' excellent inerting and dielectric properties make it a viable replacement for higher GWP fluids such a..