Polymer Property : Thermal Conductivity = 0.0295 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.00425 W/m-K

@Pressure 10.0 MPa
0.0295 BTU-in/hr-ft²-°F

@Pressure 1450 psi
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel
Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivit..