Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Excelfrax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivity by reducing the heat transfer due to convection and conduction. Welded in polyethylene (PE) film under vacuum, the low thermal conductivity values of Excelfrax 200 VIP are due to low inner pressure. Its insulating value provides equipment designers and users with advantages such as design flexibility by reducing insulation space requirements in appliances, increased volume in commercial and domestic refrigerators, reduction in package size and weight of insulated shipping containers, increased volume for cargo in insulated shipping containers, and allows for longer shipping times/distances for temperature-controlled transportation systems.Typical ApplicationsResidential and industrial refrigeratorsInsulated packaging/shipping containersRefrigerated trucks/transportation systemsMarine/Recreational Vehicle refrigeratorsVending machinesCold storage unitsInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.186 g/cc
0.00671 lb/in³
Mechanical Properties Metric English Comments
Compression Set 7.0 %

@Pressure 0.100 MPa
7.0 %

@Pressure 14.5 psi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.800 J/g-°C

@Temperature 32.0 - 800 °C
0.191 BTU/lb-°F

@Temperature 89.6 - 1470 °F
Thermal Conductivity 0.00363 W/m-K

@Pressure <=0.00100 MPa
0.0252 BTU-in/hr-ft²-°F

@Pressure <=0.145 psi
0.00366 W/m-K

@Pressure 0.100 MPa
0.0254 BTU-in/hr-ft²-°F

@Pressure 14.5 psi
0.00375 W/m-K

@Pressure 1.00 MPa
0.0260 BTU-in/hr-ft²-°F

@Pressure 145 psi
0.00425 W/m-K

@Pressure 10.0 MPa
0.0295 BTU-in/hr-ft²-°F

@Pressure 1450 psi
0.00484 W/m-K

@Pressure 25.0 MPa
0.0336 BTU-in/hr-ft²-°F

@Pressure 3630 psi
Maximum Service Temperature, Air 90.0 °C
194 °F
Recommended Operating Temperature
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended Operating Temperature
Shrinkage 0.030 %

@Temperature 50.0 °C
0.030 %

@Temperature 122 °F
All sides, long term
0.10 %

@Temperature 100 °C
0.10 %

@Temperature 212 °F
All sides, long term
Component Elements Properties Metric English Comments
SiC 15 %
15 %
SiO2 80 %
80 %
Descriptive Properties Value Comments
Cold Crushing Strength (MPa) 0.5
DIN 51067 / DIN 53421
Color Silver
Heat Flux (W/m2-K) 0.187
<.001
0.188
0.1
0.193
1
0.219
10
0.249
25
Other Inorganics (%) 5