Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP6015F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIQ10015ER UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP EQX10030R UV Polypropylene, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 63.0 °C @Load 5.001 kg |
145 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized Information provided by Polykemi AB |