Polymer Property : Vicat Softening Point = 245 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 245 °C

@Load 1.02 kg
473 °F

@Load 2.25 lb
120°C/hour; ISO 306
Ineos ABS Triax® 3158 ABS + Polyamide Blend (DAM), PA66/ABS Pellets (filled)
Triax® 3158 is a PA+ABS-Blend and on-line paintable (195°C). It has very high heat resistance, reduced moisture, improved impact strength, and a low coefficient of linear thermal expansion. It..
Vicat Softening Point 245 °C

@Load 1.02 kg
473 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terblend® N 3158 ASA / PA, 9% Mineral filled
Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.High ..
Vicat Softening Point 245 °C

@Load 0.999 kg
473 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
Characteristics: 30% glass fibre filled