Thermal Properties Metric English Comments
Vicat Softening Point 180 °C

@Load 0.999 kg
356 °F

@Load 2.20 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 3000 ABS / Nylon 6 Blend
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri..
Vicat Softening Point 180 °C

@Load 0.999 kg
356 °F

@Load 2.20 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1616 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, good dimensional stabil..
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM PA 6 Polyamide 6
Characteristics: medium viscosity, general purpose
Vicat Softening Point 180 °C

@Load 5.10 kg
356 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..