Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 165 °C @Load 1.00 kg |
329 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 165 °C @Load 1.02 kg |
329 °F @Load 2.25 lb |
ISO 306 |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Vicat Softening Point | 165 °C @Load 5.10 kg |
329 °F @Load 11.2 lb |
cond.; ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |