Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 151 °C @Load 1.00 kg |
304 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 151 °C @Load 1.00 kg |
304 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANFILL Injection CPC35051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 151 °C @Load 1.00 kg |
304 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Vicat Softening Point | 151 °C @Load 1.02 kg |
304 °F @Load 2.25 lb |
ISO 306 |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Vicat Softening Point | 151 °C @Load 1.00 kg |
304 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer Information provided by Polykemi AB |