Polymer Property : Vicat Softening Point = 140 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP EIP2012 F Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.001 kg
140 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC T10030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 60.0 °C

@Load 5.10 kg
140 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion
Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha..