Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS7 F20 PBT/ASA Blend, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 5.001 kg |
284 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC M75R Polycarbonate, Steam Resistant Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH K20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH K5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 5.001 kg |
284 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S75R Polycarbonate Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.02 kg |
284 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ ED230HP Polypropylene TPO Compound Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Vicat Softening Point | 140 °C @Load 1.02 kg |
284 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Vicat Softening Point | 140 °C @Load 1.02 kg |
284 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate.. |
|||
Vicat Softening Point | 140 °C @Load 1.02 kg |
284 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Vicat Softening Point | 140 °C @Load 0.999 kg |
284 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 10% glass fiber reinforcementGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 140 °C @Load 0.999 kg |
284 °F @Load 2.20 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND PSA 8500 V0 Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, excellent light resistance, high impact resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.. |
|||
Vicat Softening Point | 140 °C @Load 5.10 kg |
284 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® Rx2435 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Vicat Softening Point | 140 - 145 °C @Load 5.00 kg |
284 - 293 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Vicat Softening Point | 140 °C @Load 5.00 kg |
284 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Vicat Softening Point | 140 - 145 °C @Load 5.00 kg |
284 - 293 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
Vicat Softening Point | >= 140 °C @Load 0.999 kg |
>= 284 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T5020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.00 kg |
284 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 140 °C @Load 1.02 kg |
284 °F @Load 2.25 lb |
ISO 306 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |