Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 122 °C @Load 5.001 kg |
252 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS8 FR UV PC/ASA, Flame Retardant, UV-Stabilized Information provided by Polykemi AB |
|||
Vicat Softening Point | 122 °C @Load 1.02 kg |
252 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Vicat Softening Point | 122 °C @Load 1.02 kg |
252 °F @Load 2.25 lb |
ISO 306 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Vicat Softening Point | 122 °C @Load 5.10 kg |
252 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |