Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 117 °C @Load 0.999 kg |
243 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 117 °C @Load 0.999 kg |
243 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 117 °C @Load 0.999 kg |
243 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |