Thermal Properties Metric English Comments
Vicat Softening Point 117 °C

@Load 0.999 kg
243 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene
ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 117 °C

@Load 0.999 kg
243 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 117 °C

@Load 0.999 kg
243 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS