Thermal Properties Metric English Comments
Vicat Softening Point 115 °C

@Load 5.001 kg
239 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP HIP15025 HC Polypropylene
Information provided by Polykemi AB
Vicat Softening Point 115 °C

@Load 1.00 kg
239 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 115 °C

@Load 5.001 kg
239 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance
Information provided by Polykemi AB
Vicat Softening Point 115 °C

@Load 1.02 kg
239 °F

@Load 2.25 lb
120°C/hour; ISO 306
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
Vicat Softening Point 115 °C

@Load 1.02 kg
239 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Novodur® HH-106 ABS
Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution
Vicat Softening Point 115 °C

@Load 1.02 kg
239 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND PSA 8500 V0 HF Flame Retardant PC / ASA Blend
Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, chlorine and bromine free, excellent light resistance, high impact resistance, excellent processabilityInformation pro..
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0420 HHT Acrylonitrile Butadiene Styrene
ABS for injection molding or extrusionVery high thermal resistance, good impact resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 115 °C

@Load 0.999 kg
239 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0460 GF Acrylonitrile Butadiene Styrene, 30% Glass Filled
ABS with 30% glass fiber reinforcementExcellent dimensional stability, low shrinkage, good impact resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim..
Vicat Softening Point 115 °C

@Load 0.999 kg
239 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good impact resistance, high gloss, good light resistance, good processabilityInformation provided by Cos..
Vicat Softening Point 115 °C

@Load 0.999 kg
239 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1515 HT Acrylonitrile Butadiene Styrene
ABS with high thermal resistanceGood melt flow rate, good impact resistance, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 115 - 118 °C

@Load 0.999 kg
239 - 244 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epiryl B PPO Polyphenylene oxide
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation ..
Vicat Softening Point 115 °C

@Load 1.00 kg
239 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
50°C/hr; ISO 306