Thermal Properties Metric English Comments
Vicat Softening Point 114 °C

@Load 5.00 kg
237 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, high thermal resistanceInformation provided by Cossa Po..
Vicat Softening Point 114 °C

@Load 0.999 kg
237 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
ABS for sheet and profile extrusionHigh impact resistance, excellent heat resistance, excellent dimensional stability and processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 114 °C

@Load 0.999 kg
237 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 114 °C

@Load 5.10 kg
237 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® T50 BBS083 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo..
Vicat Softening Point 114 °C

@Load 5.10 kg
237 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® XT5010 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Easy processing• Low..
Vicat Softening Point 114 °C

@Load 5.00 kg
237 °F

@Load 11.0 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..