Polymer Property : Maximum Service Temperature, Air = 94.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 94.4 °C
202 °F
Heat Distortion, Annealed; ASTM D648
Total PSI 960E Polystyrene
Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids ..