Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 94.4 °C | 202 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |