Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 549 °C | 1020 °F | Continuous |
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C). |
|||
Maximum Service Temperature, Air | 549 °C | 1020 °F | Continuous |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |