Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name Lamp-Coat™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC)
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Solids Content 31.9 %
31.9 %
by volume
35.8 %
35.8 %
by weight
Volatile Organic Compounds (VOC) Content 731 g/l
731 g/l
Viscosity 300 - 400 cP
300 - 400 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
79.5 microns
3.13 mil
estimated wet film thickness
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 549 °C
1020 °F
Continuous
Flash Point 48.0 °C
118 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 48.9 °C
50.0 - 120 °F
Application Temperature
Cure Time 4.80 min
0.0800 hour
Air Set prior to curing
12000 min

@Temperature 30.0 °C
200 hour

@Temperature 86.0 °F
10 mins at 900°F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Silver
Dry Film Coverage ft2/gal 512
at 1 mil
Thinner Ethanol