Polymer Property : Maximum Service Temperature, Air = 478 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 248 °C
478 °F
Heat distortion temperature, load unknown; ASTM D648
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Maximum Service Temperature, Air 248 °C
478 °F
Dry
3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer
Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.Product Features:Combines good..