Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 423 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Plenco 08122 Polyester BMC, Compression Molded
PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Copyright © lookpolymers.com All Rights Reserved