Polymer Property : Maximum Service Temperature, Air = 421 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 216 °C
421 °F
Heat Resistance; ASTM D570D
Plenco 4349 Phenolic, Granular, Injection Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Maximum Service Temperature, Air 216 °C
421 °F
Heat Resistance; ASTM D570D
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Maximum Service Temperature, Air 216 °C
421 °F
Heat Resistance; ASTM D570D
Plenco 4568 Phenolic, Granular, Compression Molded
PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl..
Maximum Service Temperature, Air 216 °C
421 °F
Henkel Hysol EA 9689 Film Adhesive
Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding