Polymer Property : Maximum Service Temperature, Air = 405 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 207 °C
405 °F
Heat Resistance; ASTM D570D
Plenco 2000 Phenolic, Granular, Compression Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Maximum Service Temperature, Air 207 °C
405 °F
Heat Resistance; ASTM D570D
Plenco 7507 Phenolic, Granular, Compression Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Maximum Service Temperature, Air 207 °C
405 °F
Heat Resistance; ASTM D570D
Plenco 4485 Phenolic, Granular, Transfer Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..