Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7507 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7507 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solutions at elevated temperature. UL recognized under component file E40654. 07507 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Water Absorption 0.41 %
0.41 %
ASTM D570
Linear Mold Shrinkage 0.0037 cm/cm
0.0037 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 72
72
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 0.76 %
0.76 %
ASTM D638
Tensile Modulus 9.40 GPa
1360 ksi
ASTM D638
Flexural Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Compressive Strength 177 MPa
25700 psi
ASTM D695
Izod Impact, Notched 0.189 J/cm
0.354 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.208 J/cm²
0.990 ft-lb/in²
ASTM D256
Impact 110
110
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 207 °C
405 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Shrinkage 0.38 %
0.38 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+13 ohm-cm
1.60e+13 ohm-cm
ASTM D247
Dielectric Constant 5.8
5.8
ASTM D150
Dielectric Strength 13.2 kV/mm
335 kV/in
Short Time; ASTM D149
Dissipation Factor 0.051
0.051
ASTM D150
Arc Resistance 183 sec
183 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638