Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 174 - 178 °C | 345 - 352 °F | Softening Range |
Huntsman HT 9664 Aromatic Amine Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: Micropulverized HT 976: 4,4' -diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°.. |
|||
Maximum Service Temperature, Air | 174 - 178 °C | 345 - 352 °F | Softening Range |
Huntsman HT 976 Aromatic Amine Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: 4,4'-diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°C. Excellent high temper.. |
|||
Maximum Service Temperature, Air | 174 °C | 345 °F | Temperature Index |
AlphaGary Megolon™ S800 Low Smoke Halogen Free A thermoplastic, halogen free, fire retardant high speed cable sheathing compound for general purpose applications. This product exhibits excellent processing characteristics including the ability t.. |