Thermal Properties Metric English Comments
Maximum Service Temperature, Air 174 - 178 °C
345 - 352 °F
Softening Range
Huntsman HT 9664 Aromatic Amine
Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: Micropulverized HT 976: 4,4' -diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°..
Maximum Service Temperature, Air 174 - 178 °C
345 - 352 °F
Softening Range
Huntsman HT 976 Aromatic Amine
Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: 4,4'-diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°C. Excellent high temper..
Maximum Service Temperature, Air 174 °C
345 °F
Temperature Index
AlphaGary Megolon™ S800 Low Smoke Halogen Free
A thermoplastic, halogen free, fire retardant high speed cable sheathing compound for general purpose applications. This product exhibits excellent processing characteristics including the ability t..