Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1830 °C | 3330 °F | Intermittent |
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |