Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1830 °C
3330 °F
Intermittent
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.