Polymer Property : Maximum Service Temperature, Air = 2950 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1620 °C
2950 °F
Continuous
Pyrotek M-14 Compressible/Insulating Boards
ApplicationsSiphon gaskets Trough and ladle linings Tundishes Mill board substitute AdvantagesResistant to chemical attack Excellent thermal shock resistance Slightly flexible Moderately compressibl..
Maximum Service Temperature, Air 1620 °C
2950 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 60 AP Dense Refractory Brick
Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime ..
Maximum Service Temperature, Air 1620 °C
2950 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 85 M Dense Refractory Brick
Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that..