Maximum Service Temperature, Air 88.0 - 204 °C
190 - 399 °F
Average value: 136 °C Grade Count:10
Overview of materials for Silicone, RTV, Construction Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values..
Maximum Service Temperature, Air 125 - 204 °C
257 - 400 °F
Average value: 136 °C Grade Count:13
Overview of materials for Chlorosulfonated Polyethylene Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val..