Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu.. |
|||
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast VIBRON 180 Dense Vibrating Refractory Castable Description: Vibron 180 is a low cement castable with an alumina bond. The material is supplied in two components. The B component is a liquid.Remarks: Indicated values apply to vibrated products.In.. |
|||
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast VIBRON 180 RAPID Dense Vibrating Refractory Castable Description: Vibron 180 Rapid is a low cement castable based on corundum with a special addition to enable a faster heating schedule. The material is supplied in two components. The B component cont.. |
|||
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast VIBRON 180 T Dense Vibrating Refractory Castable Description: Vibron 180 T is a low cement castable, based on tabular alumina.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Maximum Service Temperature, Air | 1870 °C | 3400 °F | |
Gouda Vuurvast CURON 185 T Dense Refractory Castable Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values .. |