Thermal Properties Metric English Comments
Maximum Service Temperature, Air 186 °C
367 °F
Heat Resistance; ASTM D570D
Plenco 2369 Phenolic, Granular, Injection Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..