Thermal Properties Metric English Comments
Maximum Service Temperature, Air 825 °C
1520 °F
Long Term
Brandenburger ISOFLEX AFV Foam
This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio..
Maximum Service Temperature, Air 825 °C
1520 °F
AGY VeTron® Glass Fiber
Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.Information provided by AGY Holding Corp.