Polymer Property : Maximum Service Temperature, Air = 142 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 142 °C
288 °F
Heat Resistance; ASTM D570D
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..