Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 00714 Melamine-Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00714 Melamine-Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E40654. 00714 is available in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D1895
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Water Absorption 0.286 %
0.286 %
ASTM D570
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 71
71
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Compressive Strength 151 MPa
21900 psi
ASTM D695
Poissons Ratio 0.31
0.31
ASTM D638
Shear Modulus 4.20 GPa
609 ksi
Calculated
Izod Impact, Notched 0.159 J/cm
0.298 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.165 J/cm²
0.785 ft-lb/in²
ASTM D256
Impact 85
85
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 142 °C
288 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.90 %
0.90 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.70e+12 ohm-cm
3.70e+12 ohm-cm
ASTM D247
Dielectric Constant 6.9
6.9
ASTM D150
Dielectric Strength 6.30 kV/mm
160 kV/in
Step by Step; ASTM D149
9.50 kV/mm
241 kV/in
Short Time; ASTM D149
Dissipation Factor 0.069
0.069
ASTM D150
Arc Resistance 186 sec
186 sec
ASTM D495
Comparative Tracking Index 575 V
575 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved