Material Notes:
Black or colors casting, resurfacing, coating, and adhesive. 100/100 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 9.6 %
9.6 %
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Processing Properties Metric English Comments
Pot Life >= 80 min
>= 80 min
Descriptive Properties Value Comments
Color Black
Viscosity High