Polymer Property : Maximum Service Temperature, Air = 117 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 47.0 °C
117 °F
Deflection Temp at unknown load
Abatron AboCast 8503-6/AboCure 8503-6 Colorless Epoxy
AboCast 8503-6/AboCure 8503-6 is a slow hardening, colorless epoxy casting compound with low viscosity used for larger castings. It allows for large castings and offers low viscosity for bubble-free..