Material Notes:
AboCast 8503-6/AboCure 8503-6 is a slow hardening, colorless epoxy casting compound with low viscosity used for larger castings. It allows for large castings and offers low viscosity for bubble-free casting because of its low viscosity and slow reactivity. Its low exotherm also allows embedding of heat-sensitive specimens. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.
Physical Properties Metric English Comments
Viscosity 200 cP
200 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Strength at Break 62.7 MPa
9100 psi
Elongation at Break 14 %
14 %
Flexural Strength 62.7 MPa
9100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 47.0 °C
117 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Pot Life 210 min

@Temperature 25.0 °C
210 min

@Temperature 77.0 °F
500 g
Descriptive Properties Value Comments
Hardening Time (min) 240-1080
Parts by Weight (pbw) 100
AboCast
40
AboCure