Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | -60.0 - 200 °C | -76.0 - 392 °F | |
SMAC BARRIER® Damping Material SMAC BARRIER® is a new material developed by SMAC to complete the range of solutions for noise reduction into an aircraft. SMAC BARRIER® is an acoustic layer designed to reduce the transmissio.. |