Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 200 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
392 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |
|||
Maximum Service Temperature, Inert | 200 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
392 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |
|||
Maximum Service Temperature, Inert | 200 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
392 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi.. |